Oxide ceramics handle heat, struggle with corrosion in reverse-flow pyrolysis petrochemical reactors

By Eileen De Guire / January 4, 2013

Cross-sectional SEM images of the corroded polycrystalline 8 mol%-YSZ coupon after testing in the reverse‐flow pyrolysis reactor for about 70 hours showing the corrosion of polycrystalline bulk material to fine-grained…