‘Low temperature’ processing with electric field assisted sintering

By Eileen De Guire / June 4, 2013

Shrinkage during electric field assisted sintering can lead to debonding and cracking, as shown this sample of 8YSZ sintered at 840°C. Credit: Kim; JACerS; Wiley. When I started writing this, I was on my way—literally, at 34,000 feet somewhere over Arizona—to the PACRIM-GOMD meeting this week in San Diego. While there I will be dropping…