Nanoindentation experiments reveal porous particle size matters for assembled material toughness

By April Gocha / January 9, 2018

After collecting extensive data, researchers at Rice University (Houston, Texas) can definitively say that, when it comes to porous nanoparticles, size matters—and, in the process, they’ve made some surprising discoveries about how size affects the materials’ intrinsic properties.