Experimental Study of the Aging and Self-Healing of the Glass/Ceramic Sealant Used in SOFCs

By / January 28, 2010

Volume 7 Issue 1, Pages 22 – 29 Wenning N. Liu, Xin Sun, Brian Koeppel, Mohammad KhaleelPublished Online: Aug 15 2009 1:43AM DOI: 10.1111/j.1744-7402.2009.02417.x ABSTRACT High operating temperatures of solid oxide fuel cells (SOFCs) require that the sealant must function at a high temperature between 600°C and 900°C and in the oxidizing and reducing environments…

Read More

Thermochemical Compatibility of a Seal Glass with Different Solid Oxide Cell Components

By / January 28, 2010

Volume 7 Issue 1, Pages 22 – 29 Kevin KendallPublished Online: Feb 23 2009 1:59PM DOI: 10.1111/j.1744-7402.2008.02350.x ABSTRACT High operating temperatures of solid oxide fuel cells (SOFCs) require that the sealant must function at a high temperature between 600°C and 900°C and in the oxidizing and reducing environments of fuel and air. This paper describes…